Utilisation of De-Oiled Bleaching Earth as Fine Filler in Light weight Foam Concrete: Material Characteristics andCuring-Dependent Strength

Authors

  • Mohd Izzat Bin Ismail Author
  • Muhd Fauzy Sulaiman Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Habib Musa Bin Mohamad Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Nelly Binti Majain Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Mohammad Radzif Bin Taharin Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Arif Luqman Bin Bacho Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Nazaruddin Bin Abdul Taha Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author
  • Eugene Soo Zhen Xiang Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia Author

DOI:

https://doi.org/10.47363/JCERT/2026(8)213

Keywords:

Curing-Dependent Strength, De-Oiled Bleaching Earth, Fine Filler, Material Characteristics

Abstract

Lightweight Foam Concrete (LFC) relies on thin cementitious walls surrounding entrained air voids, and their continuity strongly influences mechanical performance. This conference study evaluates De-Oiled Bleaching Earth (DOBE) as a fine filler in an LFC trial formulation containing 3.00 kg cement, 3.70 kg DOBE, 0.25 kg silica fume, 5.00 L water and 150 mL concentrated concrete foaming agent. Raw DOBE was characterised using X-Ray Fluorescence (XRF), X-Ray Diffraction (XRD), Field-Emission Scanning Electron Microscopy with Energy-Dispersive X-Ray Analysis (FESEM-EDX), and Atomic Force Microscopy (AFM). Brick specimens were subjected to steam curing at 70 °C for 48 h followed by 24 h ambient cooling, or to water and openair curing for 28 days. XRF identified SiO2 as the dominant oxide (50.79 wt.%), with CaO, Fe2O3 and Al2O3 also present. FESEM and AFM revealed irregular agglomerates and non-uniform nanoscale topography, with Ra = 0.971 nm and Rq = 1.24 nm. EDX showed predominantly siliceous-aluminous particles together with a local Ca-rich region. Steam-cured specimens achieved 5.75 MPa, compared with 5.42 MPa for water curing and 5.14 MPa for open-air curing. The results support DOBE as a physically and chemically heterogeneous fine filler and indicate that steam curing can accelerate strength development in DOBE-containing LFC.

Author Biographies

  • Mohd Izzat Bin Ismail

    Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia

  • Muhd Fauzy Sulaiman, Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia

    Muhd Fauzy Sulaiman, Faculty of Engineering, Universiti Malaysia Sabah, Kota Kinabalu, Malaysia.

Downloads

Published

2026-10-20